CL-FLJ268

This is applicable when there is a problem of missed plating due to excessive aluminum content in the zinc bath.

This is applicable when there is a problem of missed plating due to excessive aluminum content in the zinc bath. Before the treatment of the flux, a pre-treatment for preventing missed plating should be carried out to solve the problem of missed plating on the workpiece.

CL-FLJ268 hot dip galvanization anti-bare-spots surface treatment agent is a light blue aqueous solution, mainly composed of water-soluble organic chelating agents, surfactants, antioxidants, activators and metal organic compounds. This product does not contain lead, cadmium, mercury, hexavalent chromium, fluorine or phosphorus, and is an environmentally friendly product. Steel treated with this product and then processed with conventional zinc chloride-ammonium chloride flux can be galvanized in zinc solution with aluminum content ranging from 0.01% to 0.15% without any missed plating.


Hunan Chuanglin New Material Technology Co., Ltd.

Address:No.1 Chuanglin Road,Wantang Industrial Park,Lukou District,Zhuzhou Hunan Province Telephone:0731-27288889 Email:hnzzcl168@126.com
Consultation Hotline

0731-27288889 0731-27288218 13307337885 18890221062

Scanning Two-Dimensional Code Sharing to Wechat